Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 224 °C | 435 °F | dry |
Henkel Hysol EA 9689 Film Adhesive Modified epoxy film adhesive with high temperature strength and long-term thermal durability. Data from 0.10 psf, 500 g/m2.Applications: Composite Bonding Metal and Honeycomb Bonding |