Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 185 °C | 365 °F | DSC; IPC-TM-650.2.4.25c |
Park Electrochemical Nelco® N5000 BT Epoxy Laminate and Prepreg The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and .. |
|||
Glass Transition Temp, Tg | >= 185 °C | >= 365 °F | DSC; IPC-TM-650.2.4.25c |
Park Electrochemical Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy The Nelco N4000-29 is a lead-free, low-CTE, high Tg multifunctional epoxy substrate which has been designed for use in standard multilayer PWB designs and today’s toughest, high-performance, lead-f.. |
|||
Glass Transition Temp, Tg | 185 °C | 365 °F | ASTM E1356 |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)
(Unverified Data**) Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest.. |
|||
Glass Transition Temp, Tg | 185 °C | 365 °F | ASTM E1356 |
Solvay Specialty Polymers Udel® M-2300 MR Polysulfone (PSU), Mold Release
(discontinued **) Udel M-2300 MR is an injection-moldable, low-color grade of polysulfone that is nearly water white in color. This material contains a mold release which aids part ejection when parts with low draft .. |
|||
Glass Transition Temp, Tg | 185 °C | 365 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific.. |
|||
Glass Transition Temp, Tg | 185 °C | 365 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Glass Transition Temp, Tg | 185 °C | 365 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties.. |
|||
Glass Transition Temp, Tg | 185 °C | 365 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP BMC 3100 is a special BMC suitable for the use in head lamp reflectors. Because of its high temperature resistance and dimensional stability as well as low coefficient of thermal expansion, complex .. |
|||
Glass Transition Temp, Tg | 185 °C | 365 °F | ASTM E1356 |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU) Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved .. |
|||
Glass Transition Temp, Tg | >= 185 °C | >= 365 °F | |
Master Bond EP45HTMED Epoxy Resists Radiation and Steam Sterilization Description: Master Bond Polymer System EP45HTMED is a two component heat cured epoxy system for high performance structural bonding, sealing, coating and casting. It is especially designed for the .. |
|||
Glass Transition Temp, Tg | >= 185 °C | >= 365 °F | |
Master Bond EP45HTND-2 Chemically Resistant, Non-Drip Epoxy Description: Master Bond EP45HTND-2 is a two component epoxy system for high performance bonding, sealing and coating. It is used for applications requiring solid temperature resistance and capable .. |
|||
Glass Transition Temp, Tg | 185 °C | 365 °F | |
Hexcel® HexPly® M21 356°F (180°C) Curing Epoxy Matrix HexPly® M21 is a new, very tough epoxy matrix that exhibits excellent damage tolerance, especially at high energy impact. It has been developed to meet the needs of the latest generation of primary.. |
|||
Glass Transition Temp, Tg | >= 185 °C | >= 365 °F | DSC; IPC-TM-650.2.4.25c |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |
|||
Glass Transition Temp, Tg | 185 - 265 °C | 365 - 509 °F | Average value: 221 °C Grade Count:4 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |