Polymer Property : Glass Transition Temp, Tg = 345 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 174 °C
345 °F
wet
Henkel Hysol EA 9689 Film Adhesive
Modified epoxy film adhesive with high temperature strength and long-term thermal durability. Data from 0.10 psf, 500 g/m2.Applications: Composite Bonding Metal and Honeycomb Bonding