Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 28.0 °C | 82.4 °F | ASTM E1545-00 |
DSM Somos® WaterClear® 10120 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10120 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
Glass Transition Temp, Tg | 28.0 °C | 82.4 °F | TM R050-25 |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |