Polymer Property : Glass Transition Temp, Tg = 265 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 265 °C
509 °F
ASTM E1356
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)  (Unverified Data**)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E..
Glass Transition Temp, Tg 265 °C
509 °F
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..
Glass Transition Temp, Tg 265 °C
509 °F
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t..
Glass Transition Temp, Tg 265 °C
509 °F
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin  (discontinued **)
Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i..
Glass Transition Temp, Tg 265 °C
509 °F
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..