Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 240 °C | 464 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N4380-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Glass Transition Temp, Tg | 240 °C | 464 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |