Polymer Property : Glass Transition Temp, Tg = 232 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 111 °C
232 °F
Eastman Eastalloy DA106 PC+PET Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Glass Transition Temp, Tg 111 °C
232 °F
Eastman Tenite 371A-08 Cellulose Acetate Propionate  (discontinued **)
8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Glass Transition Temp, Tg 111 °C
232 °F
ASTM D-4065
CMT Materials REN Shape® 470 Tooling Board, Modeling Board, Adhesive Products
CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume prod..
Glass Transition Temp, Tg 111 °C
232 °F
Armstrong A-1/E Epoxy Adhesive
A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El..