Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = 228 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 228 °C
442 °F
ISO 11357-1/-2
BASF Ultrason® E 3010 MR UN PESU
Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat..