Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 222 °C | 432 °F | ISO 11357-1/-2 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |