Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 198 °C | 388 °F | DMTA |
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix HexPly® M18 has been developed to fulfill the requirements of the aerospace industry for primary structures using standard manufacturing processes. The matrix has improved properties which allow ea.. |