Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 67.0 °C | 153 °F | Ultimate Tg |
Tra-Con Tra-Bond 216C04 Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | 67.0 °C | 153 °F | TM R050-25 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |