Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -76.0 - -10.0 °C | -105 - 14.0 °F | Average value: -42.9 °C Grade Count:43 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |