Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 133 °C | 271 °F | Wet |
Hexcel® HexPly® F263 Epoxy Resin HexPly® F263 is a structural, heat resistant epoxy resin formulated for excellent translation of high modulus carbon fiber properties in typically aerospace applications. HexPly® F263 is a high te.. |
|||
Glass Transition Temp, Tg | 133 °C | 271 °F | dry |
Henkel Hysol EA 9686 Film Adhesive Second generation, moisture resistant, toughened 250°F / 121°C curing film with service performance to 300°F / 149°C. Excellent for composite or metal bonding. Data from .060 psf, 300 g / m2.App.. |