Polymer Property : Glass Transition Temp, Tg = 12.7 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -10.7 °C
12.7 °F
DSC (-80°C+100°C)
Objet FullCure® 970 Tango Black Resin for Rapid Prototyping
Information provided by American Precision Prototyping, LLC