Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 46.8 °C | 116 °F | |
3M Novec™ 2708 Electronic Grade Coating 3M™ Novec™ 2708 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a low viscosity solution of a 8 wt% fluorochemical acrylic polyme.. |
|||
Glass Transition Temp, Tg | 46.8 °C | 116 °F | |
3M Novec™ 2704 Electronic Grade Coating 3M™ Novec™ 2704 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 4 wt% fluoropolymer carried .. |