Thermal Properties Metric English Comments
Glass Transition Temp, Tg 112.4 °C
234.3 °F
with 3K Resin with 3K Twill TR30 Carbon Fiber; ASTM D7028-07
Zyvex Performance Materials Arovex™ HT 250 Nano-Engineered Composite Prepreg System
Arovex® HT 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (1..