Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | ASTM D1329 |
Seals Eastern 5053 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | ASTM D3418 |
DSM Biomedical BioSpan® SPU Segmented Polyether Polyurethane (SPU) The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.The .. |
|||
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | 10°C/min |
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | 10°C/min |
Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 35 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | 10°C/min |
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | 10°C/min |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |
|||
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | Cured property; JMTP P200 |
Aptek 2100-A/B Urethane Encapsulant and/or Potting Compound General purpose encapsulant and potting compound. Outstanding hydrolytic stability. Excellent adhesion to components/circuit boards. Low modulus, low stress. Field proven for military and space appl.. |
|||
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | Cured property; ASTM E831-86 |
Aptek 7503LM-PMF UV Urethane Conformal Coating UV-cured, low modulus, shadow cures under components. Excellent adhesion without primer. Repairable. Qualified to MIL-I-46058C, types UR and AR. Castable version – UVIKOTE 7504 LM-PMF.Information p.. |
|||
Glass Transition Temp, Tg | -65.0 °C | -85.0 °F | Cured property; ASTM E831-86 |
Aptek 7504LM-PMF UV Urethane Coating/Encapsulant UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR.Information provided by Aptek Laboratories, .. |
|||
Glass Transition Temp, Tg | -65.0 - -50.0 °C | -85.0 - -58.0 °F | Average value: -58.6 °C Grade Count:7 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |