Thermal Properties Metric English Comments
Glass Transition Temp, Tg -85.0 °C
-121 °F
ASTM E-1356
Dynasol Solprene® 9320 Multi-branched Thermoplastic Rubber (Multi-branched SBS)
Solprene® 9320 is a 68/32 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It has a non-staining FDA approved antioxidant system for food contact applications and it is essen..