Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -22.0 °C | -7.60 °F | ASTM D3417 |
REXtac Rextac® RT 2215 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance and flexibility, short open time, and good wettingApplications: Component of hot melt adhes.. |
|||
Glass Transition Temp, Tg | -22.0 °C | -7.60 °F | ASTM D3417 |
REXtac Rextac® RT 2280 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance and flexibility, short open time, and high viscosityApplications: Component of hot melt adh.. |
|||
Glass Transition Temp, Tg | -22.0 °C | -7.60 °F | ASTM D3417 |
REXtac Rextac® RT 2732 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good tack, and very long open timeApplications: Component of hot mel.. |
|||
Glass Transition Temp, Tg | -22.0 °C | -7.60 °F | ASTM D3417 |
REXtac Rextac® RT 3280 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Temperature resistance, high melt viscosity, and hardnessApplications: Component of modified bitumen roofing.. |
|||
Glass Transition Temp, Tg | -22.0 °C | -7.60 °F | ASTM D3417 |
REXtac Rextac® RT 1215 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance, short open time, and excellent wetting propertiesApplications: Lamination of reinforced tapes and prot.. |
|||
Glass Transition Temp, Tg | -22.0 °C | -7.60 °F | ASTM D3417 |
REXtac Rextac® RT 1230 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance, short open time, and excellent wetting propertiesApplications: Lamination of reinforced tapes and prot.. |
|||
Glass Transition Temp, Tg | -22.0 °C | -7.60 °F | |
Styron DL 2212LA Carboxylated SB Performance Features: General purpose, high adhesion to paper and olefin substrates, low stiffness, water resistanceApplications: General Purpose AdhesiveLatin America/South AmericaInformation provi.. |
|||
Glass Transition Temp, Tg | -22.0 °C | -7.60 °F | DSC |
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |