Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -28.1 - -20.9 °C | -18.6 - -5.62 °F | Zeon Test #1273 |
Zeon Chemicals HyTemp® AR72LF AR Polyacrylate Elastomer HyTemp AR72LF contains acrylic esters with a small percentage of chlorine cure site monomer. Vulcanizates have excellent oil, heat, and compression set resistance with good low temperature.Excellent.. |