Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -43.0 °C | -45.4 °F | DSC, 10°C/min; ISO 11357-2 |
Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H92S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Glass Transition Temp, Tg | -43.0 °C | -45.4 °F | |
Sorbothane Polyurethane Damping Material, 50 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m.. |
|||
Glass Transition Temp, Tg | -43.0 °C | -45.4 °F | |
Zeon Chemicals Hydrin® T3000 Polyepichlorohydrin Elastomer Hydrin T3000 is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high oil, fuel and solvent resistance. Compounds using Hydrin T3000 typically exhibit excellent low and high te.. |
|||
Glass Transition Temp, Tg | -43.0 °C | -45.4 °F | |
Zeon Chemicals Hydrin® T3000L Polyepichlorohydrin Elastomer Hydrin T3000L is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high oil, fuel and solvent resistance. Compounds using Hydrin T3000L typically exhibit excellent low and high .. |
|||
Glass Transition Temp, Tg | -43.0 °C | -45.4 °F | |
Zeon Chemicals Hydrin® T3000LL Polyepichlorohydrin Elastomer Hydrin T3000LL is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high oil, fuel and solvent resistance. Compounds using Hydrin T3000LL typically exhibit excellent low and hig.. |
|||
Glass Transition Temp, Tg | -43.0 °C | -45.4 °F | Pellet sample |
BASF Elastollan® 1180A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Glass Transition Temp, Tg | -43.0 °C | -45.4 °F | Pellet sample |
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Glass Transition Temp, Tg | -43.0 °C | -45.4 °F | DSC |
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane Features: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and b.. |