Polymer Property : Glass Transition Temp, Tg = -33.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -33.9 °C
-29.0 °F
ASTM D3417
REXtac Rextac® RT 5219 Amorphous Polyalphaolefin (APAO)
Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, ethylene copolymer, and FDA compliantFeatures: High ethylene level and low crystallinityApplications: Component of modified ..