Glass Transition Temp, Tg -31.2 °C
-24.2 °F
By DSC
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
Glass Transition Temp, Tg -31.2 °C
-24.2 °F
By DSC
DuPont Vamac® DP Activator OC Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..