Polymer Property : Glass Transition Temp, Tg = -22.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -22.2 °C
-8.00 °F
DSC, 10ºC/min; DIN 51.007
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1..
Glass Transition Temp, Tg -22.2 °C
-8.00 °F
ASTM D1329
Seals Eastern 7265D Fluorocarbon-Elastomer
Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc.