Polymer Property : Glass Transition Temp, Tg = -162 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -108 °C
-162 °F
Cured property; TMA
Aptek 2710A/B Low modulus silicone adhesive
Low modulus silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space grade; Electrostatically Discharging (ESD)APTEK 2710-A/B is a two component, black, low modulus, thixotropic, s..