Polymer Property : Glass Transition Temp, Tg = -11.2 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta..
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2351-85AE elastomer is a polyether hybrid specialty polyurethane elastomer compound which combines excellent resistance to fuels and oils with good hydrolytic stability and high damping..
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
Mallard Creek Polymers ROVENE® 4305 SBR Latex
ROVENE® 4305 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This non-woven and textile binder offers outstanding..
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
Mallard Creek Polymers ROVENE® 5005 SBR Latex
ROVENE® 5005 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This paper saturant offers good water and solvent re..
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
Mallard Creek Polymers Rovene® 6119 Styrene-Acrylic Emulsion
Applications: Rovene® 6119 is a low glass transition temperature styrene-acrylic polymer that offers flexibility during movement of the substrate and water resistance. Rovene® 6119 also exhibi..
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
Mallard Creek Polymers ROVENE® 8305 SBR Emulsion
ROVENE® 8305 is a 50% bound styrene, high gel content hot polymerized styrene – butadiene emulsion. Compatibility with commercial tackifier resin emulsions is excellent, as is filler toleran..
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
DSC
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf..
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
DSC
Lubrizol Estane® MVT 90AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 90AF3 TPU is a 90A aromatic polyether-based thermoplastic polyurethane.Features: High moisture vapor transmission, good physical properties and elasticity, free of organo-tin comp..
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
DSC
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
DSC
Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Description: PELLETHANE® 2101-85A offers good low temperature properties, fast cycle time, and good hydrolytic stability. Applications include: seals, gaskets, animal tags, molding applications, ho..