Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.09 - 2.16 J/g-°C @Temperature 10.0 - 290 °C |
0.261 - 0.516 BTU/lb-°F @Temperature 50.0 - 554 °F |
Average value: 1.58 J/g-°C Grade Count:2 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |