Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.04 J/g-°C | 0.488 BTU/lb-°F | |
Styron CALIBRE™ 200 4 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Specific Heat Capacity | 2.04 J/g-°C | 0.488 BTU/lb-°F | |
Styron CALIBREâ„¢ 5101 15 Polycarbonate, 10% Glass Reinforced CALIBRE 5101 is a 10% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5101 resin exhibits high modulus and excellent dimensional stability. CALIBRE 5101 .. |