Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.71 J/g-°C | 0.409 BTU/lb-°F | Melt |
Covestro Makroblend® DP 2-7655 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD10(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |