Polymer Property : Specific Heat Capacity = 1.407 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.407 J/g-°C
0.3363 BTU/lb-°F
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..