Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.20 - 1.40 J/g-°C @Temperature 40.0 - 260 °C |
0.287 - 0.335 BTU/lb-°F @Temperature 104 - 500 °F |
Average value: 1.30 J/g-°C Grade Count:14 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |