Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.246 J/g-°C @Temperature 1093 °C |
0.2978 BTU/lb-°F @Temperature 1999 °F |
|
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator Fibermax Mat is a high-temperature, flexible mat product that is lightweight (1.5 lb/ft3 density) and highly resilient. It is composed entirely of Fibermax polycrystalline mullite fibers to produce.. |
|||
Specific Heat Capacity | 1.246 J/g-°C @Temperature 1093 °C |
0.2978 BTU/lb-°F @Temperature 1999 °F |
|
Unifrax Fibermax® Needled Blanket Fibermax® Needled Blankets are high temperature, light weight and flexible products manufactured from polycrystalline mullite fiber that can be exposed to temperatures up to 1600°C (2912°F). Fib.. |