Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.9991 J/g-°C | 0.2388 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |