Thermal Properties Metric English Comments
Specific Heat Capacity 0.946 - 0.962 J/g-°C
0.226 - 0.230 BTU/lb-°F
Average value: 0.960 J/g-°C Grade Count:15
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..