Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.740 J/g-°C | 0.177 BTU/lb-°F | calculated |
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Specific Heat Capacity | 0.740 J/g-°C | 0.177 BTU/lb-°F | |
Schott N-SF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.740 J/g-°C | 0.177 BTU/lb-°F | |
Schott N-BAF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.740 J/g-°C @Temperature 100 - 200 °C |
0.177 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Alunit® Aluminum Nitride Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its .. |
|||
Specific Heat Capacity | 0.740 J/g-°C @Temperature 100 °C |
0.177 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
CoorsTek Hot Pressed Aluminum Nitride Aluminum Nitride Advantages: High heat dissipation with thermal conductivity of 170 W/m K Non-toxic alternative to BeO Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors H.. |