Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.690 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.690 J/g-°C

@Temperature 0.000 - 50.0 °C
0.165 BTU/lb-°F

@Temperature 32.0 - 122 °F
Momentive Performance Materials Type 254 Fused Quartz Tubing
A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen ..
Specific Heat Capacity 0.690 J/g-°C
0.165 BTU/lb-°F
Schott N-BAK2 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.690 J/g-°C
0.165 BTU/lb-°F
Schott N-BALF4 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.690 J/g-°C
0.165 BTU/lb-°F
Schott N-FK51A Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.690 J/g-°C
0.165 BTU/lb-°F
Schott N-KZFS11 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.690 J/g-°C
0.165 BTU/lb-°F
Schott N-SF6 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.690 J/g-°C
0.165 BTU/lb-°F
Schott N-SF6HT Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.690 J/g-°C
0.165 BTU/lb-°F
ASTM-E1269
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate)
Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua..
Copyright © lookpolymers.com All Rights Reserved