Polymer Property : Specific Heat Capacity = 0.545 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 2.28 J/g-°C
0.545 BTU/lb-°F
Solvay Chemicals DIGLYCEROL
Diglycerol is a clear viscous liquid very similar to glycerol. It has a higher molecular weight than glycerol and is less volatile. It is water soluble and can be combined with aqueous systems.EINEC..
Specific Heat Capacity 2.28 J/g-°C
0.545 BTU/lb-°F
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers