Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.23 J/g-°C | 0.533 BTU/lb-°F | |
Dow Tyril® 880B SAN TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.Data provided b.. |