Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.11 J/g-°C | 0.504 BTU/lb-°F | |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Specific Heat Capacity | 2.11 J/g-°C | 0.504 BTU/lb-°F | |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Specific Heat Capacity | 2.11 J/g-°C | 0.504 BTU/lb-°F | |
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |