Polymer Property : Specific Heat Capacity = 0.500 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.350 - 0.500 J/g-°C
0.0837 - 0.120 BTU/lb-°F
Alliance A-5S Alnico Magnetic Material
Specific Heat Capacity 0.350 - 0.500 J/g-°C
0.0837 - 0.120 BTU/lb-°F
Alliance A-8S Alnico Magnetic Material
Specific Heat Capacity 0.350 - 0.500 J/g-°C
0.0837 - 0.120 BTU/lb-°F
Alliance A-6S Alnico Magnetic Material
Specific Heat Capacity 0.350 - 0.500 J/g-°C
0.0837 - 0.120 BTU/lb-°F
Alliance A-2S Alnico Magnetic Material