Polymer Property : Specific Heat Capacity = 0.4680 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.958 J/g-°C
0.4680 BTU/lb-°F
Melt
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Specific Heat Capacity 1.958 J/g-°C
0.4680 BTU/lb-°F
Melt
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..