Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.454 J/g-°C | 0.109 BTU/lb-°F | |
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-.. |
|||
Specific Heat Capacity | 0.454 J/g-°C @Temperature 100 °C |
0.109 BTU/lb-°F @Temperature 212 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |