Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C | 0.105 BTU/lb-°F | |
Special Metals INCOLOY® alloy 908 INCOLOY® alloy 908 (UNS N09908) is an age-hardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue cr.. |
|||
Specific Heat Capacity | 0.439 J/g-°C | 0.105 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel Description: S692/S693 MICROCLEAN are high-sulfur and low sulfur versions of high-carbon PM M4 high speed steel that is produced using state-of-the-art “Generation 3” powder processing technology... |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 20.0 °C |
0.105 BTU/lb-°F @Temperature 68.0 °F |
|
Carlson 904L Austenitic Stainless Steel General Description904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a w.. |
|||
Specific Heat Capacity | 0.439 J/g-°C | 0.105 BTU/lb-°F | |
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Specific Heat Capacity | 0.439 J/g-°C | 0.105 BTU/lb-°F | |
Carpenter Chrome Core® 12-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |