Thermal Properties Metric English Comments
Specific Heat Capacity 1.79 J/g-°C
0.428 BTU/lb-°F
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene  (discontinued **)
STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins...