Polymer Property : Specific Heat Capacity = 0.425 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.78 J/g-°C
0.425 BTU/lb-°F
Melt
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade
Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content