Thermal Properties Metric English Comments
Specific Heat Capacity 0.415 J/g-°C
0.0992 BTU/lb-°F
Carpenter Chrome Core® 8 Alloy
Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen..
Specific Heat Capacity 0.415 J/g-°C
0.0992 BTU/lb-°F
Carpenter Chrome Core® 8-FM Alloy
Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen..