Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.414 J/g-°C | 0.0989 BTU/lb-°F | |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
Specific Heat Capacity | 0.414 J/g-°C @Temperature 100 °C |
0.0990 BTU/lb-°F @Temperature 212 °F |
|
Schmolz + Bickenbach MoldMAX® SC Copper Alloy Description: Brush Wellman’s MoldMAX® SC is a high conductivity copper mold alloy with good strength. MoldMAX® SC is used as blow mold cavities, injection mold cores and cavities and hot .. |