Thermal Properties Metric English Comments
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 100 °C
0.0968 BTU/lb-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.405 J/g-°C

@Temperature 21.0 °C
0.0968 BTU/lb-°F

@Temperature 69.8 °F
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..