Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.584 J/g-°C | 0.3786 BTU/lb-°F | |
Materion E20 Beryllium/BeO Composite, 20 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |