Polymer Property : Specific Heat Capacity = 0.318 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.33 J/g-°C
0.318 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® FL403 PC
Various weight reductions at 0.250"" wall. UV-resistant. Impact resistant, Superior processing, excellent surface. UL94 V-0/5V at 0.125"".